Posted by Tom Clarkeover 3 years ago
HIT-HY 200 A Resin performance in low temperatures

How is HIT-HY 200 A resin curing times impacted by low temperatures (approx -5 degrees celcius) and will this impact the time required to wait until performing a pull test on the anchor?

HIT-HY 200-A,Low temperature

1 Reply
Posted by Ask HILTI Teamover 3 years ago

Thank you for your question . I've attached the ETA for the HY200A for standard anchor rod elements. You are correct that the base material temperature will affect the minimum cure time and consequently you will need to wait until this time period has lapsed. Table B7 within the ETA provides this information along with the minimum temperature of the foil pack.